Sv-08X19H10G2BU
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| OST 24.300.04-91 |
65.117–70.55 |
< 0.45 |
1.6–2.2 |
18–20 |
9–10.5 |
< 0.018 |
< 0.1 |
< 0.015 |
0.85–1.35 |
< 0.25 |
Information on suppliers
Properties
| Property |
| Density: 7.82 g / cm3 |