Sv-08H1DYu
For the manufacture of cold-drawn wire, intended for automatic and manual welding of atmospheric — corrosion-resistant steel type 10HNDP.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Materials for welding and soldering | Steel welding wire |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-1148 - 75 | 97.21–98.46 | 0.12–0.35 | 0.3–0.6 | 0.9–1.2 | 0.2–0.35 | 0.02–0.12 | < 0.035 | < 0.1 | < 0.035 |