Sv-08N60G8M7T (EP705)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ti, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-1836-76 |
21.355–28.7 |
< 0.4 |
7–10 |
0.3–0.6 |
52.655–65.345 |
< 0.025 |
< 0.1 |
< 0.02 |
6–7.5 |
Information on suppliers
Properties
| Property |
| Density: 8.57 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |