Sv-1
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Zr, % |
Al, % |
Ce, % |
OE, % |
| GOST Р 56031-14 |
< 0.04 |
< 0.1 |
93.24–95.6 |
< 0.02 |
< 0.05 |
1–1.8 |
< 0.01 |
0.4–1 |
< 0.01 |
3–3.7 |
< 0.03 |