St-10 ha

Welding cold drawn wire of low carbon steel welding (surfacing), and the manufacture of electrodes

Classification

Country Section Category
CIS, Russia, Ukraine Materials for welding and soldering Steel welding wire

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Ni, % P, % C, % S, % N, %
GOST 2246-70 97.855–98.9 < 0.06 1.1–1.4 < 0.2 < 0.3 < 0.03 < 0.12 < 0.025 < 0.01

Information on suppliers

Eigenschaften

Eigenschaft
Dichte: 7,86 g / cm³

Standards

Standard Description
GOST 2246-70