Sv-10GN1MA
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
Al, % |
As, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| TU 14-1-2203-77 |
94.64–96.57 |
0.15–0.35 |
1.1–1.5 |
< 0.3 |
< 0.25 |
1.5–1.8 |
< 0.1 |
< 0.05 |
< 0.08 |
< 0.02 |
0.08–0.12 |
< 0.02 |
0.6–0.75 |
< 0.02 |
Information on suppliers
Properties
| Property |
| Density: 7.88 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |