St-10GSMT
Welding cold drawn wire of stainless steel, for welding (welding) and the manufacture of electrodes
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Materials for welding and soldering | Steel welding wire |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2246-70 | 96.685–98.27 | 0.4–0.7 | 1–1.3 | < 0.3 | 0.05–0.12 | < 0.3 | < 0.03 | 0.08–0.14 | < 0.025 | 0.2–0.4 |
Information on suppliers
Properties
| Property |
|---|
| Density: 7.83 g / cm3 |
Standards
| Standard | Description |
|---|---|
| GOST 2246-70 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |