Sv-10H16N25G5AM6
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Materials for welding and soldering | Steel welding wire |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Cu, % | Ni, % | Al, % | P, % | C, % | S, % | Nb, % | Mo, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 42.447–50.92 | < 0.3 | 4–5.5 | < 0.05 | 15–17 | < 0.25 | 24–27 | < 0.1 | < 0.018 | 0.08–0.12 | < 0.015 | < 0.1 | 6–7 | < 0.1 |
Information on suppliers
Properties
| Property |
|---|
| Density: 8.13 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |
| N | % | Nitrogen |