Sv-10X19H11M4F (EP647)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-2921-80 |
59.935–65.33 |
0.6–1 |
1.5–2 |
18–20 |
10–11.5 |
0.7–1.1 |
< 0.02 |
0.07–0.12 |
< 0.025 |
3.8–4.3 |
Information on suppliers
Properties
| Property |
| Calculated Properties Density: 7.87 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |