Sv-10X21H11FT
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
| TU 14-1-3638-83 |
60.71–66.55 |
0.7–1.2 |
1.2–2 |
20.5–22.5 |
0.1–0.35 |
10–11.5 |
0.9–1.6 |
< 0.02 |
0.05–0.1 |
< 0.02 |
Information on suppliers
Свойства
| Свойство |
| Вычисляемые свойства Плотность: 7.74 г/см3 |