Sv-10X2M
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| OST 26-291-94 |
95.89–97.7 |
0.12–0.37 |
0.4–0.7 |
1.3–1.7 |
< 0.25 |
< 0.3 |
< 0.03 |
0.08–0.13 |
< 0.03 |
0.4–0.6 |
Information on suppliers
Properties
| Property |
| According to TU 14-1-2219-77 Note Failed state |
| First quality category Note Mechanical properties are not standardized |
| Calculated Properties Density: 7.85 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |