Sv-10X3M1A

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Wrought Aluminum Alloys

Chemical composition

Standard Fe, % Si, % Mn, % Co, % Cr, % Ti, % Cu, % Ni, % V, % Al, % P, % C, % S, % Mo, % N, %
OST 26-291-94 93.786–96.08 0.2–0.35 0.9–1 < 0.02 2.1–2.5 0.05–0.25 < 0.6 < 0.2 < 0.3 < 0.05 < 0.006 0.07–0.12 < 0.006 0.6–0.8 < 0.012

Information on suppliers

Eigenschaften

Eigenschaft
Berechnete Eigenschaften Dichte: 7,84 g / cm3

Standards

Standard Description
OST 26-291-94
TU 14-1-4914-90

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Co % Cobalt
Cr % Chrome
Ti % Titan
Cu % Copper
Ni % Nickel
V % Vanadium
Al % Aluminium
P % Phosphorus
C % Carbon
S % Sulfur
Mo % Molybdenum
N % Nitrogen