Sv-10HG2SMF
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | As, % | P, % | C, % | S, % | Mo, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 0805-001-18486807-99 | 95.395–97.17 | 0.5–0.7 | 1.2–1.6 | 0.7–0.9 | < 0.04 | < 0.2 | < 0.2 | 0.15–0.3 | < 0.05 | < 0.04 | < 0.025 | 0.08–0.12 | < 0.02 | 0.2–0.4 | < 0.01 |
Note: The chemical composition of the weld metal
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 7.82 g / cm3 |
| Note For hardfacing, creating a wear-resistant coating for the restoration of railway transport parts |
Standards
| Standard | Description |
|---|---|
| TU 0805-001-18486807-99 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| As | % | Arsenic |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| N | % | Nitrogen |