Sv-10HGSN2MT
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-2203-77 |
94.35–96.37 |
0.4–0.7 |
1–1.3 |
0.4–0.7 |
0.05–0.1 |
< 0.25 |
1.5–2 |
< 0.03 |
0.08–0.14 |
< 0.03 |
0.2–0.4 |
Information on suppliers
Свойства
| Свойство |
| Вычисляемые свойства Плотность: 7.85 г/см3 |