St-10HM

Welding cold drawn wire of stainless steel, for welding (welding) and the manufacture of electrodes

Classification

Country Section Category
CIS, Russia, Ukraine Materials for welding and soldering Steel welding wire

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Ni, % P, % C, % S, % Mo, %
GOST 2246-70 96.715–98.05 0.12–0.3 0.35–0.6 0.9–1.2 < 0.3 < 0.03 0.08–0.13 < 0.025 0.5–0.7

Information on suppliers

Eigenschaften

Eigenschaft
Berechnete Eigenschaften Dichte: 7,86 g / cm3

Standards

Standard Description
GOST 2246-70

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Cr % Chrome
Ni % Nickel
P % Phosphorus
C % Carbon
S % Sulfur
Mo % Molybdenum