St-10HMFA
Welding cold drawn wire of stainless steel, for welding (welding) and the manufacture of electrodes
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Materials for welding and soldering | Steel welding wire |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | V, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2246-70 | 96.42–97.9 | 0.12–0.3 | 0.35–0.6 | 0.9–1.2 | < 0.3 | 0.15–0.3 | < 0.025 | 0.08–0.13 | < 0.025 | 0.5–0.7 |
Information on suppliers
Свойства
| Свойство |
|---|
| Вычисляемые свойства Плотность: 7.86 г/см3 |
Standards
| Standard | Description |
|---|---|
| GOST 2246-70 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |