Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
W, % |
| TU 14-1-2683-79 |
94.055–96.38 |
0.8–1.2 |
0.5–0.8 |
0.8–1.2 |
< 0.15 |
0.8–1.2 |
0.05–0.15 |
< 0.015 |
0.17–0.22 |
< 0.01 |
0.5–1 |
Information on suppliers