Sv-28H3SNMVFA-VD (EP835-VD)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| TU 14-1-2683-79 |
91.33–93.45 |
0.9–1.2 |
0.5–0.8 |
2.8–3.2 |
< 0.1 |
0.9–1.2 |
0.05–0.15 |
< 0.012 |
0.25–0.3 |
< 0.008 |
0.35–0.5 |
0.8–1.2 |
Information on suppliers
Свойства
| Свойство |
| Вычисляемые свойства Плотность: 7.91 г/см3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |