Sv-H11N60M23
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Materials for welding and soldering | Steel welding wire |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|
| < 0.5 | < 1 | 9.5–13 | 60.86–69 | < 0.02 | < 0.1 | < 0.02 | 21.5–24.5 |
Information on suppliers
Properties
| Property |
|---|
| Weld Temperature: 800 ° C; Ultimate Strength: 118 MPa |
| After heat treatment Note Exposure at 700 ° C, 16 hours |
| Temperature: 800 ° C; Ultimate Strength: 157.6 MPa |
| Calculated Properties Density: 8.97 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |