Saint-HN23MTYUR
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
|
< 0.5 |
< 1 |
9.5–13 |
60.86–69 |
< 0.02 |
< 0.1 |
< 0.02 |
21.5–24.5 |
Information on suppliers
Properties
| Property |
| According to TU 14-1-997-2012 Note Mechanical properties are not standardized |
| According to TU 14-1-997-2012 Note Mechanical properties: as agreed |
| Calculated Properties Density: 8.11 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |