St.-HN28VMAB-VD
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
N, % |
W, % |
| TU 14-1-997-2012 |
34.255–47.7 |
< 0.6 |
< 0.005 |
< 1.5 |
19–22 |
< 0.2 |
25–30 |
< 0.2 |
< 0.02 |
< 0.1 |
< 0.02 |
0.7–1.3 |
2.8–3.5 |
< 0.3 |
4.8–6 |
Information on suppliers
Properties
| Property |
| According to TU 14-1-997-2012 Note Mechanical properties are not standardized |
| According to TU 14-1-997-2012 Note Mechanical properties: as agreed |
| Calculated Properties Density: 8.66 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
| W |
% |
Tungsten |