St.-HN38BB
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Al, % |
Ce, % |
P, % |
C, % |
S, % |
Nb, % |
W, % |
| TU 14-1-997-2012 |
30.38–40.94 |
< 0.8 |
< 0.7 |
20–23 |
< 0.2 |
35–39 |
< 0.5 |
< 0.05 |
< 0.03 |
0.06–0.12 |
< 0.02 |
1.2–1.7 |
2.8–3.5 |
Information on suppliers
Properties
| Property |
| According to TU 14-1-997-2012 Note Mechanical properties are not standardized |
| According to TU 14-1-997-2012 Note Mechanical properties: as agreed |
| Calculated Properties Density: 8.42 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| W |
% |
Tungsten |