St.-HN70Yu
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Ba, % |
Al, % |
Ce, % |
P, % |
C, % |
S, % |
| TU 14-1-997-2012 |
< 1 |
< 0.8 |
< 0.3 |
26–29 |
< 0.07 |
65.073–71.2 |
< 0.1 |
2.8–3.5 |
< 0.03 |
< 0.015 |
< 0.1 |
< 0.012 |
Information on suppliers
Properties
| Property |
| According to TU 14-1-997-2012 Diameter: <2 mm; Temporary resistance: <1670 MPa |
| Diameter:> 2 mm; Temporary resistance: <1080 MPa |
| Calculated Properties Density: 8.18 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Ba |
% |
Barium |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |