St.-HN75MBTY
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| TU 14-1-997-2012 |
< 3 |
< 0.8 |
< 0.4 |
19–22 |
0.35–0.75 |
< 0.07 |
68.498–77.6 |
0.35–0.75 |
< 0.02 |
< 0.1 |
< 0.012 |
0.9–1.3 |
1.8–2.3 |
Information on suppliers
Properties
| Property |
| According to TU 14-1-997-2012 Diameter: <2 mm; Temporary resistance: <1670 MPa |
| Diameter:> 2 mm; Temporary resistance: <1080 MPa |
| Calculated Properties Density: 8.45 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |