SvA99
For the manufacture of welding wire.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Cu, % | Zn, % | Al, % | Примеси, % | OE, % |
|---|---|---|---|---|---|---|---|
| GOST 4784-97 | < 0.003 | < 0.003 | < 0.003 | < 0.003 | > 99.977 | < 0.01 | < 0.001 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 | |
| GOST 7871-75 | GOST 7871 - 75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| OE | % | Other items |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |