Svamc
For the manufacture of welding wire.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|
| GOST 7871-75 | 0.3–0.5 | 0.2–0.4 | < 0.05 | 1–1.5 | < 0.2 | < 0.1 | 97.25–98.5 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Wire | GOST 7871-75 | 100 |
Analogues
| Germany | USA |
|---|---|
| AG1 | AA3103 |
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 | |
| GOST 7871-75 | GOST 7871 - 75 |
| GOST Р 57517-2017 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |