SvAMg3
For the manufacture of welding wire.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|
| GOST 4784-97 | < 0.5 | 0.5–0.8 | 3.2–3.8 | 0.3–0.6 | < 0.05 | < 0.2 | 94.05–96 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| S-AlMg3 | AA5154 |
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 | |
| GOST 7871-75 | GOST 7871 - 75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |