SvAMg5
For the manufacture of welding wire.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 4784-97 | < 0.4 | < 0.4 | 0.002–0.005 | 4.8–5.8 | 0.5–0.8 | 0.1–0.2 | < 0.05 | < 0.2 | 92.145–94.598 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| S-AlMg4,5Mn | AA5183 |
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 | |
| GOST 7871-75 | GOST 7871 - 75 |