T-MF
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Sn, % | Mg, % | Bi, % | Mn, % | Co, % | Cr, % | Cu, % | Ni, % | Sb, % | Al, % | Te, % | Pb, % | As, % | Cd, % | Ga, % | Ag, % | In, % | Hg, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 5.0E-5 | < 6.0E-5 | < 6.0E-5 | < 2.0E-5 | < 5.0E-5 | < 5.0E-5 | < 0.0001 | > 2.0E-5 | < 5.0E-5 | < 0.0001 | < 5.0E-5 | 99.9991–99.99998 | < 6.0E-5 | < 1.0E-5 | < 3.0E-5 | < 2.0E-5 | < 2.0E-5 | < 5.0E-5 | < 0.0001 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Te | % | Tellurium |
| Pb | % | Lead |
| As | % | Arsenic |
| Cd | % | Cadmium |
| Ga | % | Gallium |
| Ag | % | Silver |
| In | % | Indium |
| Hg | % | Mercury |