T12 (VT1-2)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | C, % | O, % | N, % | H, % | OE, % |
|---|---|---|---|---|---|---|---|---|
| GOST 2171-90 | < 1.5 | < 0.15 | > 97.49 | < 0.1 | < 0.3 | < 0.15 | < 0.01 | < 0.3 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 2171-90 | GOST 2171-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Ti | % | Titan |
| C | % | Carbon |
| O | % | Oxygen |
| N | % | Nitrogen |
| H | % | Hydrogen |