T14K8
For the processing of materials by cutting: Rough turning with uneven sections cut and continuous cutting, Finishing and finish turning with interrupted cuts; rough milling of solid surfaces; reaming cast and forged holes, rough reaming and other similar kinds of processing carbon and alloy steels.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Hard sintered alloys |
Chemical composition
| Standard | WC, % | Co, % |
|---|---|---|
| GOST 3882-74 | > 92 | < 8 |
Information on suppliers
Analogues
| Germany |
|---|
| HS123 |
Standards
| Standard | Description |
|---|---|
| GOST 3882-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| WC | % | Wolfram carbide |
| Co | % | Cobalt |