T15K6
For the processing of materials by cutting: Poluchernovogo turning in continuous cutting, finish turning with interrupted cuts, tapping trademarks cutters and rotating heads, Finishing and finish milling of solid surfaces, reaming and boring pretreated holes, finishing reaming, deployment, and other similar types of processing carbon and alloy steels.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Hard sintered alloys |
Chemical composition
| Standard | WC, % | Co, % |
|---|---|---|
| GOST 3882-74 | > 94 | < 6 |
Information on suppliers
Analogues
| Germany |
|---|
| HS123 |
Standards
| Standard | Description |
|---|---|
| GOST 3882-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| WC | % | Wolfram carbide |
| Co | % | Cobalt |