T32 (VT32)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Cr, % |
Ti, % |
V, % |
Al, % |
C, % |
O, % |
Mo, % |
N, % |
H, % |
ET, % |
| GOST 2171-90 |
0.5–2 |
0.5–2 |
80.385–89.5 |
0.5–2 |
2–4 |
< 0.1 |
< 0.15 |
7–9 |
< 0.05 |
< 0.015 |
< 0.3 |