TG-150
Hardness TG-150 (GOST 17667) HB 10 -1 = 150 MPa
starting material for the production of semi-finished products made of titanium and its alloys; first — quality category
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Titanium, titanium alloys | Sponge titanium |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Ni, % | C, % | O, % | Cl, % | N, % |
|---|---|---|---|---|---|---|---|---|
| GOST 17746-96 | < 0.2 | < 0.03 | < 99.45 | < 0.04 | < 0.03 | < 0.1 | < 0.12 | < 0.03 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 17746-96 | |
| DSTU 3079-95 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ti | % | Titan |
| Ni | % | Nickel |
| C | % | Carbon |
| O | % | Oxygen |
| Cl | % | Chlorine |
| N | % | Nitrogen |