TG-TV
starting material for the production of semi-finished products made of titanium and its alloys; first — quality category
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Titanium, titanium alloys | Sponge titanium |
Chemical composition
| Standard | Fe, % | Ti, % | C, % | Cl, % | N, % |
|---|---|---|---|---|---|
| GOST 17746-96 | < 1.9 | < 97.75 | < 0.1 | < 0.15 | < 0.1 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 17746-96 | |
| DSTU 3079-95 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Ti | % | Titan |
| C | % | Carbon |
| Cl | % | Chlorine |
| N | % | Nitrogen |