Tl000
For the product ingots and pellets, used in various industries
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Thallium |
Chemical composition
| Standard | Fe, % | Sn, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | Cd, % | Ag, % | In, % | Tl, % | Hg, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 18337 - 95 | < 0.0001 | < 0.0001 | < 3.0E-5 | < 5.0E-6 | < 5.0E-5 | < 2.0E-5 | < 0.0001 | < 3.0E-5 | < 3.0E-6 | < 3.0E-5 | < 0.0001 | > 99.999392 | < 4.0E-5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 18337 - 95 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |
| Cd | % | Cadmium |
| Ag | % | Silver |
| In | % | Indium |
| Tl | % | Thallium |
| Hg | % | Mercury |