Tl1
For the product ingots and pellets, used in various industries
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Thallium |
Chemical composition
| Standard | Fe, % | Cu, % | Zn, % | Pb, % | Cd, % | Tl, % |
|---|---|---|---|---|---|---|
| GOST 18337 - 95 | < 0.001 | < 0.003 | < 0.003 | < 0.01 | < 0.003 | > 99.98 |