TN20
For the processing of materials by cutting: Finish turning and roughing in continuous cutting carbon low-alloy structural steel, nonferrous metals, copper-based, low-alloyed nickel alloys, gray cast iron and polyethylene. Finishing and roughing face milling of cast iron Medium to finish turning and milling of carbon and alloyed steel with HRC 30−42, chromium and corrosion-resistant and heat-resistant steel with a tensile strength of 600−800 MPa
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Hard Sintered Tungsten Free Alloys |
Chemical composition
| Standard | TiC, % | Ni, % | Nb, % | Mo, % |
|---|---|---|---|---|
| GOST 26530-85 | 78.9–99.95 | < 15 | 0.05–0.1 | < 6 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 26530-85 |