TS3S
for the production of hot-rolled anodes used for galvanizing parts electroplated
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Zinc is the primary |
Chemical composition
| Standard | Fe, % | Sn, % | Cu, % | Zn, % | Pb, % | As, % | Cd, % |
|---|---|---|---|---|---|---|---|
| GOST 3640-94 | < 0.05 | < 0.04 | < 0.02 | < 98.5 | < 1.4 | < 0.01 | < 0.2 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 3640-94 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Pb | % | Lead |
| As | % | Arsenic |
| Cd | % | Cadmium |