TC6
The hardness of the sheet TC6 after quenching and aging HB 10 -1 = 341 — 444 MPa .
for the production of cavitation-resistant products; class pseudo-β structure
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Titanium, titanium alloys |
Wrought Titanium Alloys |
Chemical composition
| Standard |
Cr, % |
Ti, % |
V, % |
Al, % |
Mo, % |
|
10–11 |
75–77 |
6–6 |
3–3 |
4–5 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Sheet |
GOST 27265-87 |
|
|
|
1580–1635 |
1520–1590 |
5.5–6 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Sheet |
|
Hardening, aging |
341–444 |
Description of chemical elements
| Element |
Units of measurement |
Description |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| Mo |
% |
Molybdenum |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |