TSAM10-2
Hardness ЦАМ10−2 HB 10 -1 = 95 — 100 MP and.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Metals and alloys |
Zinc Wrought Alloys |
Chemical composition
| Standard |
Mg, % |
Cu, % |
Zn, % |
Al, % |
|
0.03–0.03 |
2–2 |
87.97–87.97 |
10–10 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
6210 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$\psi$$, % |
Treatment |
|
|
|
|
|
350–450 |
15–20 |
45–60 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
|
|
|
950–1000 |
Description of chemical elements
| Element |
Units of measurement |
Description |
| Mg |
% |
Magnesium |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Al |
% |
Aluminium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$\psi$$ |
% |
Reduction in cross section on fracture |