TSAM10-5L (TsAM10-5)
Hardness TsAM10−5L (GOST 21437−95) HB 10 -1 = 100 MPa.
casting podschipnikov and sleeves of different units
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Zinc antifriction alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Cu, % | Zn, % | Al, % | Pb, % | Cd, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 21437-95 | < 0.15 | < 0.1 | < 0.01 | 0.03–0.06 | 4–5.5 | 81.8–86.62 | 9–12 | < 0.03 | < 0.02 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\epsilon_L$$, % | Treatment |
|---|---|---|---|---|---|---|---|
| GOST 21437-95 | 245 | 0.4 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 21437-95 | 1000 |
Standards
| Standard | Description |
|---|---|
| GOST 21437-95 | |
| DSTU 2774-94 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
| Pb | % | Lead |
| Cd | % | Cadmium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |