The hardness of the CMP, Sheet (GOST 18239) HB 10 -1 = 50 MP and.
for the production of sheets used for the manufacture of printing forms of high single-stage etching.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Zinc Wrought Alloys |
Chemical composition
| Standard | Fe, % | Sn, % | Mg, % | Cu, % | Zn, % | Al, % | Pb, % | Cd, % |
|---|---|---|---|---|---|---|---|---|
| GOST 18326-87 | < 0.004 | < 0.001 | 0.03–0.06 | < 0.001 | 99.815–99.897 | 0.06–0.1 | < 0.006 | < 0.003 |
Information on suppliers
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Sheet | GOST 18326-87 | 500 |
Standards
| Standard | Description |
|---|---|
| GOST 18326-87 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
| Pb | % | Lead |
| Cd | % | Cadmium |