TT10K8B (TT10K8-B)
For the processing of materials by cutting: Rough-finishing and some brands of hard materials, stainless austenitic steels, low-magnetic steel and heat-resistant steels and alloys, including titanium.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Hard sintered alloys |
Chemical composition
| Standard | WC, % | TiC, % | Co, % |
|---|---|---|---|
| GOST 3882-74 | > 82 | > 7 | < 8 |
Information on suppliers
Analogues
| Germany |
|---|
| HS420 |
Standards
| Standard | Description |
|---|---|
| GOST 3882-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| TiC | % | Titanium carbide |
| WC | % | Wolfram carbide |
| Co | % | Cobalt |