UONI-13 / N1-BK
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| GOST 33258-15 |
53.115–60.84 |
< 0.5 |
< 1.4 |
30–33 |
7–9 |
< 0.035 |
0.06–0.12 |
< 0.03 |
1.8–2.4 |
0.3–0.4 |