US-1
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Bi, % |
Cu, % |
Zn, % |
Sb, % |
Pb, % |
As, % |
| TU 48-6-98-86 |
< 0.003 |
0.13–0.18 |
< 0.015 |
0.05–0.07 |
< 0.0015 |
2.3–2.8 |
96.7505–97.38 |
0.14–0.18 |