V3K
Production of ingots and cast rods intended for further melting in the production of shaped castings; for building up valves for internal combustion engines and other parts with similar requirements.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Co, % | Cr, % | Ni, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|
| OST 1-90127 - 85 | < 2 | 2–2.75 | 51.88–64 | 29–32 | < 3 | 1–1.3 | < 0.07 | < 2 | 4–5 |