V48P
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Zr, % | Al, % | Cd, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 5.9466 - 88 | < 0.2 | < 0.15 | 1.35–1.8 | 0.2–0.4 | 0.05–0.12 | 0.3–0.6 | 4.5–5.1 | 0.07–0.2 | 91.08–93.48 | 0.05–0.2 | < 0.05 | < 0.1 |
Note: Zr > 0.10, Cd, Be: by agreement
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 5.9466 - 88 |