V65Sh
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Al, % |
Pb, % |
As, % |
OE, % |
ET, % |
| GOST 4784-97 |
< 0.2 |
< 0.25 |
0.15–0.3 |
0.3–0.5 |
< 0.1 |
3.9–4.5 |
< 0.1 |
93.735–95.65 |
< 0.15 |
< 0.015 |
< 0.05 |
< 0.1 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| OE |
% |
Other items |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |