V95B
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
OE, % |
ET, % |
| GOST 17232-99 |
< 0.5 |
< 0.5 |
1.8–2.8 |
0.2–0.6 |
0.1–0.25 |
< 0.05 |
1.4–2 |
5–7 |
< 0.1 |
86.05–91.5 |
< 0.05 |
< 0.1 |
Information on suppliers
Analogues
| Germany |
European Union |
USA |
| AlZnMgCu1.5 DIN 1725 Part 1 |
P-AlZn5.8MgCuCr |
QQ-A-250/12 AMS |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| OE |
% |
Other items |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |